Abstract

For further research on durability of concrete material under salt frozen conditions in cold area, the non air-entraining concrete with water-binder ratio of 0.4 and 0.28, air-entraining concrete with water-binder ratio 0.28 and the air content 7.0% are studied respectively. The fractal dimension of three kinds of concrete pore at different pore diameter range were determined by MIP(mereury intrusion porosimetry) before and after salt freezing and were studied in a comparative way. The research shows that the fractal dimension of pore diameter at range of 50nm ~ 550nm after salt freezing changed remarkably, namely salt frozen process has greater influence on pore within this range. Objectively the pore within this range in concrete suffered supercooled water osmotic pressure is the greatest. In addition, the total porosity reduced after salt freezing injury while fractal dimension changed more obviously. The fractal dimension of concrete pore could be a good reflection of concrete structure after salt freezing injury, showing that the diameter at 50nm ~ 550nm after salt frozen injury coarsening is obvious. Thus the fractal dimension of diameter within this range can be used as a key parameters after salt freezing injury.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.