Abstract
The pH variations of Mg, Zn and Al solutions to which had been added the rare earth metals Nd, Pr and Y were observed in 3.5 wt.% NaCl with respect to high energy mechanical ball milling effects. Mg was directly dissolved and exhibited a pH value of 10.5. On the other hand, Zn and Al needed to be saturated for a certain amount of time. The addition of rare earth metals played a role in increasing the pH with low reduction potentials. Additionally, mechanical ball milling provided high energy to Mg + x wt.% Zn + 0.5 wt.% Nd mixture by fracturing fragmentation of metals, which led to an increase in the pH when the mixture was immersed in 3.5 wt.% NaCl. The addition of Zn to Mg + 0.5 wt.% Nd caused a higher pH than when Mg + 0.5 wt.% Nd alone was added.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.