Abstract
An attempt has been made to study the pretreatment of sulfidic refractory gold ore with pyrolusite. The influences of various parameters were studied to optimize the conditions. The optimum leaching conditions were pyrolusite/gold ore mass ratio of 3.0, H2SO4concentration of 3.0 M, temperature of 100°C, particle size of 45μm, stirring speed of 200 rpm. After the pretreatment, gold and silver were exposed, these made the extraction of the precious metal in the gold ore much easier.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.