Abstract

The chemical bath deposition approach was used to arrange PbS and PbS coated with Ag thin layer thin films. PbS film was deposited at room temperature using thiourea and lead chloride as precursors. After the PbS film had been deposited, it was immersed in Ag precursors for 60 minutes at 50 C to coat its surface. In this study, we looked at absorbance in the 400-1000 nm range. The direct and indirect bandgaps were estimated using the Tauc method and yielded values between 1.3 and 1.45 eV. It resulted in increasing in bandgaps after coating with of Ag layer.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.