Abstract

Deformation of austenite containing 0.85 pct C is shown to significantly increase the ten-sile strength of bainite formed during subsequent transformation. Quantitative metallo-graphic measurements indicate that strengthening is due primarily to an increased dislo-cation density in the ferrite and reduced carbide size, with consequent finer distribution, compared with the bainite formed from undeformed austenite. It is also shown that de-formed austenite transforms to upper bainite at temperatures at least as low as 200°C due to enhanced nucleation and/or growth at slip band heterogeneities generated by the defor-mation process while the only effect on the formation of lower bainite is a retardation of the transformation and reduction of ferrite plate size.