Abstract

This paper is concert about the mechanical property of high strength and high toughness titanium alloy BTi-6554 (Ti-6Cr-5Mo-5V-4Al) bars. The results show that: in β-phase zone solid solution + aging treatment condition, the strength and fracture toughness of the alloy at room temperature can reach a higher level while inα+β)-phase solution + aging treatment condition, the plastic property is relatively high. Compared with Ti-1023 and VT22 alloy bars produced by the similar processing procedure, the alloy shows improved properties combined in strength and toughness. BTi-6554 is a new type of titanium alloy with high structural efficiency, and has a good prospect for commercial and application.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.