Abstract

The kinetics of Fe2TiO4 reduction to FeTiO3 + Fe were studied using CO-CO2 gas mixtures with fO2 measured by a solid ceramic (calcia-zirconia) oxygen electrolyte cell. Isothermal rate studies at 900 C suggest that the mechanism of Fe2TiO4 reduction is one of nucleation and growth, where the growth stage may be controlled by the diffusion of the reactant through the product layer or volume diffusion. The activation energy for the growth stage of the process was determined to be 46 plus or minus 4 kcal/mole.