Abstract

The kinetics of hot-pressing for undoped and donor-doped BaTiO3 of high purity have been studied at 1050‡ C and at 2.3 to 27.6 MPa in an oxidizing atmosphere. The stress exponent and grain size exponent of the densification rate are indicative of control of densification by a grain boundary diffusion mechanism. The activation enthalpy (∼400 kJ mol−1) for the densification process has been measured over the range of 1050 to 1 200‡ C. No significant influence of the donor is observed on the densification of BaTiO3 until the late stages of sintering.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.