Abstract
In the present work, four different PVC formulations, designed for outdoor applications, were submitted to artificial accelerated ageing under xenon light, without and with spray of water, and to natural exposure. The influence of the combined action of water and radiation was evaluated by means of surface analysis using XPS, SEM and colourimetry, permitting comparison of the results obtained under different exposure conditions. Results show that a long preliminary period of irradiation (∼2000 h) before the exposure to water increases the resistance of PVC surfaces to weather conditions. The role of that initial irradiation period is to create an erodable layer made of shrunk “PVC” that had lost most of its chlorine atoms and, thence, creating a network of cracks. That layer loses easily adhesion to deeper layers due to erosive action of water spray. The more perfect uncovered surface is better at resisting the effect of radiation.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.