Abstract
The recrystallization texture, grain boundary character distribution (GBCD) and their influence on the stress corrosion cracking and intergranular corrosion of 2024 aluminum alloy were investigated. Results showed that the texture of Specimen A1 is characterized by the retained coldrolling texture; while Specimen A3 has strong recrystallized cube texture and high frequencies of CSL grain boundaries (especially S7), which shows high stress corrosion and intergranular corrosion resistance.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.