Abstract

This paper reports on the compatibility of waste rubber as binder for M2 High Speed Steel injection moulding. The feedstock was prepared at a powder loading of 65 vol.% using 22μm M2 High Speed Steel powder and the binders consisting of 55wt.% paraffin wax, 21wt.% polyethylene, 14wt.% waste rubber and 10wt.% stearic acid. The specimens were then sintered in vacuum and 95%N2/5%H2 atmosphere. The sintering in vacuum atmosphere occurred within a temperature range from1200°C to 1260°C, whilst the 95%N2/5%H2 atmosphere was carried out within a temperature range from 1220°C to 1300°C. The effects of the sintering atmosphere and temperature on the physical properties, mechanical properties and microstructure were investigated.