Abstract

In this work, oxidation of silicon carbide particles (SiCp) at elevated temperature and its influence on the interface layer and thermal conductivity of SiCp/ZL101 composites prepared using pressure infiltration process were investigated respectively. It is found that initial temperature for the oxidation of SiCp is about 850 °C, and that the oxidation increment of SiCp and the thickness of SiO2 layer increase with the increase in pre-oxidation temperature and time, when the oxidized temperature exceeds 1100 °C, or the duration time exceeds 2 h at 1100 °C, a small amount of ablation will take place on the SiCp, as well as the oxidized layer has some loss. The formation of SiO2 layer can provide certain interface reactions with interface layers (3.1–6.36 μm), and the higher the thickness of SiO2 layer, the thicker the interface layer in SiCp/Al composites. However, the thickness of SiO2 layer is more than 5.9 μm, which is not benefit for the formation of interface layer. With the increase in the thickness of interface layer, thermal conductivity declines, but is not linear.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.