Synthesis of graphene oxide (GO) material with variations in permanganate/graphite ratio has been carried out. This research purposes to study the impact of increasing oxidizing agents to graphite on the chemical structure and properties of the GO material produced. All GOs were synthesized using the improved Tour method with three variations of permanganate/graphite ratios of 5, 6, and 7. The results obtained include GO-5, GO-6, and GO-7, respectively, having a d spacing value of 0.843; 0.891; 0.894 nm by XRD analysis and 0.768; 0.756; 0.772 nm by SAED analysis. Based on the FTIR data, all GO materials bring up the peaks of oxygen-functionalized carbon absorption such as O–H, C–H sp3, C=O, C–O–C of ether and ester, and C-OH for carboxylic acids and alcohols. The oxidation levels (O/C ratio taken from EDX data) of GO-5, GO-6, and GO-7 are 0.67, 0.88, and 1.50, respectively. SEM images display the appearance of an exfoliated layer with a wrinkled and irregular surface. TEM images show thin and transparent layers. The main peaks with the highest absorbance at the wavelength around 230-240 nm, meanwhile the band gap energy produced was 3.53; 3.71; 3.55 eV for GO-5, GO-6, and GO-7, respectively.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.