Abstract

The influence of the oxygen concentration and temperature on the UV-degradationchemistry of polyethylene is described. The degradations are characterized by measuring the oxygen uptake, the formation of CO and CO 2, the FT-IR spectra and the mechanical properties. At high temperatures (40–50 °C) an increase in the oxygen pressure (air versus 100% oxygen atmosphere) leads to a decrease of IR detectable products and to a higher amount of reacted oxygen necessary to cause mechanical failure. However, at low temperatures (29 °C) the influence of oxygen pressure is negligible. The results are explained assuming that the initiation of the photo-degradation is due to charge transfer complexes.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.