Abstract

The tensile behaviour of linear polyethylene was examined over a wide range of temperatures. Samples were prepared from low and medium molecular weight polymer with different morphologies, by varying the initial crystallization conditions. It was found that the temperature of the ductile-brittle transition was markedly different for different samples. In particular, low molecular weight polymer crystallized at a low degree of of supercooling, showed brittle behaviour over most of the temperature range, with a ductile-brittle transition near to room temperature. Rapidly quenched material, where the degree of supercooling is high, showed a very low ductile-brittle transition temperature, especially in high molecular weight polymer. The reasons for these differences in behaviour are discussed both at a phenomenological level and in terms of known structural differences between the different materials examined.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.