Abstract
The influence of mold material on cooling curve, solidification parameters, and micro-hardness were investigated. Al–6wt.% Si in clay and stainless steel mold was directionally solidified using vertical Bridgman type furnace. The samples were heated up to 700°C at 1.9°C/s heat rate, held for 60 minutes, cooled, and withdrawn at 40 µm/s. The results show that the increasing of thermal conductivity by 72% affects cooling curve shape, solidification parameters, and micro-hardness. Furthermore, comparative evaluation of the exponent value of the function of micro-hardness to distance and micro-hardness to growth rate also have been made to proposed the range of exponent value for each mold material.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
More From: IOP Conference Series: Materials Science and Engineering
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.