The influence of mold material on cooling curve, solidification parameters, and micro-hardness were investigated. Al–6wt.% Si in clay and stainless steel mold was directionally solidified using vertical Bridgman type furnace. The samples were heated up to 700°C at 1.9°C/s heat rate, held for 60 minutes, cooled, and withdrawn at 40 µm/s. The results show that the increasing of thermal conductivity by 72% affects cooling curve shape, solidification parameters, and micro-hardness. Furthermore, comparative evaluation of the exponent value of the function of micro-hardness to distance and micro-hardness to growth rate also have been made to proposed the range of exponent value for each mold material.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.