Abstract

To assess the effect of modeling liquid on the microhardness of single-shade universal composites. A total of 60 disk-shaped samples were prepared in six groups [Omnichroma (OM), Essentia Universal (EU), Vittra APS Unique (VA), OM + Signum, EU + Signum, and VA + Signum] for surface microhardness measurements. Samples were stored in a coffee solution for 7 days and after that bleached with an Office bleaching agent (Total Blanc Office). Surface microhardness was measured for baseline, after staining, and after bleaching. A two-way analysis of variance test was used for statistical analysis (P < 0.05). In terms of microhardness, there is a statistically significant difference (P < 0.05) between the two categories with and without modeling liquid. The alterations in microhardness measurements at baseline, after staining, and after bleaching are statistically significant (P < 0.05). The Essentia groups showed the lowest microhardness findings at all measurement times. Microhardness values decreased significantly more when EU was applied along with modeling liquid than when it was not applied at different intervals. Modeling liquid affects the microhardness of single-shade composites. Microhardness is reduced when modeling liquid is used for all three single-shade universal composite resins at three different times.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.