Abstract The performance of catalysts from the platinum group and Cu-based catalysts were compared in the dimethyl ether (DME) steam reforming reaction. Without acidic oxides, Cu-based catalysts formed undesired CH4 via a direct decomposition of DME into methoxy (–OCH3) and methyl (–CH3) groups, followed by the hydrogenation of the methyl group to CH4. However, in the presence of acidic oxides such as Al2O3, practically no CH4 was produced. Therefore we speculate that the MeOH formed on the acidic sites moves onto Cu and is adsorbed as a methoxy group without the co-formation of a methyl group, preventing the formation of CH4 and leading to an even higher yield of H2. Pt/Al2O3 and Ru/Al2O3 showed a relatively high DME conversion, although the undesired production of CH4 was quite high, irrespective of the presence of acidic sites. A high CH4 selectivity can be explained in terms of a high methanation activity. The catalyst formed from CuMn2O4 spinel oxide mixed with Al2O3 showed higher activity and greater durability than commercial CuZnAl catalysts mixed with Al2O3. By replacing Al2O3 with H-ZSM5, the CuMn2O4 spinel oxide showed a further increase in activity resulting in up to 100% conversion even under 300 °C. We attribute this very high activity at relatively low temperature to both the high DME hydration activity of H-ZSM5 and the high MeOH steam reforming activity of CuMn2O4 spinel oxide.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.