Gold electrode is preferable in extreme environments, but few reports focus on gold electrode for LTCC application. In this article, CaO–B2O3–SiO2 glass powder used in the gold paste with different particle size was prepared. The sintering shrinkage behavior of CaO–B2O3–SiO2 green tapes and gold paste were investigated. The blisters of gold electrode and corresponding mechanism during sintering process were studied. The sheet resistivity and wire bonding strength of gold electrode were connected with glass particle size strongly. When the D50 of CaO–B2O3–SiO2 glass powder was 2.61 μm, the wire bonding performance of gold electrode was excellent, of which the average strengths and standard deviation of wire bonding were 10.30 g and 0.66 g, respectively. These results would have a positive effect on guiding the select of glass particle size in gold paste.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.