Abstract
Abstract It has been demonstrated with examples that, for the occurrence of stress corrosion cracking (SCC), time-dependent parameters as well as critical stress levels are highly important. Therefore, certain ideas that have developed concerning the differentiation between SCC and corrosion fatigue must be revised. When cyclic loading is involved, SCC, corrosion fatigue, and fatigue are successively encountered as the frequency or strain rate is increased, and such forms of material damage are therefore predominant in particular frequency ranges.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.