Abstract

Au nanoparticles supported on MgAl-LDHs has been synthesized by coprecipitation method, gold colloid routs as well as intercalation and assembly method respectively. The influence of the above different preparation methods on the activity of the gold catalysts for CO oxidation was investigated, and the phase and gold particle size distribution of the catalysts were analyzed by XRD and TEM respectively. The results show that 100% conversion of CO on the fresh prepared gold catalysts synthesized by gold colloid routs and intercalation assembly method can be achieved at room temperature when the catalysts were activated at 473K for 2h in the air. The gold particle size distribution was range from 2nm to 7nm.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.