Platinum and silicon have been found deposited on the palladium cathode during the electrolysis of a 0.1 M LiOD solution with a platinum anode in a glass cell. Various techniques including surface analysis, cyclic voltammetry, and electrochemical permeation were used to study the surface deposits, electrochemical deuterium-sorption behavior, and permeation rate of deuterium into palladium, respectively. It was shown that palladium cathodes were contaminated by platinum and silicon deposits after a certain period of electrolysis. These deposits could affect the electrochemical processes during electrolysis. The contamination may be a cause of the sporadic results reported in [open quotes]cold fusion[close quotes] research. 18 refs., 15 figs.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.