Abstract

This study analyzed how the compositional variability of dimension stone residues influences the characteristics of rustic porous ceramic tiles. The specimens were prepared by adding 20 wt% of dimension stone residue to the clay and sintered at 1000 °C for 1 h. The testing assays performed were physical properties and structural analysis through scanning electron microscopy. The results indicate that water absorption was lower (~9% to 14%) in samples containing silicate residues compared to carbonate residues (~16%). Apparent porosity of ~21% to 25% and shrinkage of 0.5% to 1.6% were measured in silicate samples while higher apparent porosity of ~30% and expansion of -0.04% were found in carbonate samples. Flexural strength and modulus of rupture were similar, ~16 MPa and ~330 N, respectively, for both sample sets. The samples containing silicate residues whose SiO2 content was between 48% and 58% and the sum of alkaline and alkaline earth oxides was less than 18% were suitable for manufacturing rustic porous ceramic tile, while residues with high SiO2 or carbonate contents impaired the properties of the ceramic bodies. Therefore, it is recommended that the dimension stone residues intended for use in ceramic tiles be previously separated according to chemical and mineralogical characteristics.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.