Abstract
The publication presents fatigue properties of cold recycled mixtures for eight combinations of binding agents (cement and bituminous emulsion). Cold recycled mixtures were evaluated in Indirect Tensile Fatigue Test (ITFT) at the temperature of 20 °C in controlled stress mode. As a function of horizontal stress, fatigue life is strongly influenced by combination of the binding agents. When fatigue life is analyzed as a function of initial horizontal strain, the difference between different combinations decreases. In all cases, the influence of a specific binding agent is more visible for combinations with lower total amounts of the two agents.
Published Version
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.