Abstract
The effect of cold working on semiconducting properties of passive film and pitting corrosion resistance of 19Cr-18Mn-2Mo-0.9N high nitrogen austenitic stainless were investigated by anodic polarization, AC impedance and capacitance measurement methods. With increasing the cold rolling deformation ranging from 0% to 60%, the passive region of high nitrogen austenitic stainless steel decreases, and the corrosion potential, EIS radius and polarization resistance all decreases. The Mott-Schottky result indicates that the pitting corrosion resistance deteriorates with increment of cold rolling deformation. The results show that the passive films formed on high nitrogen austenitic stainless steel with different cold rolling deformation behave as n-type semiconductors. With increasing the cold rolling deformation grade, the donor density (ND) increases, but the thickness of the space-charge layer (W) decreases. The decreasing of the thickness of space-charge layer with increment of cold rolling deformation is attributed to the inceasing defect which deteriorates the stability of the passive film.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have