Abstract

The truck bias tyre bead wire coating is improved, by adjusting the rubber system, reduce the bead wire wrapped filler, appropriately increasing the amount of carbon black, and using resorcinol-formaldehyde donor-silica and cobalt salt adhesion system, the strength and adhesion property of bead wire coating were improved, bead burst and the prick-out of bead wire were decreased, the bad ratio of tire caused by bead problems was reduced from 1.3% to below 0.1%, significantly improve the actual service life of tyre.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.