Effect of the loading amount of Fe over ion-exchanged Fe-MFI catalysts on the catalytic performance of N2O reduction with NH3 was investigated, and the results indicated that the turnover frequency (TOF) was almost constant in the Fe/Al range between 0.05 and 0.40. The activity of N2O+NH3 reaction was much lower than that of N2O+CH4 reaction over Fe-MFI (Fe/Al=0.40), and the preadsorption of NH3 decreased drastically the activity of N2O+CH4 reaction. The temperature-programmed desorption (TPD) of NH3 showed the formation of stronger acid sites on Fe-MFI (Fe/Al=0.24 and 0.40), and the amount of the acid sites agrees well with the desorption amount O2 in O2-TPD in the low temperature range. The acid sites gave a 3610cm−1 peak (Brønsted acid) in FTIR observation. These results suggest that the acid sites were formed on the bridge oxide ions in binuclear Fe species. Adsorbed NH3 on the strong acid sites inhibited N2O dissociation, which can be related to the low activity of N2O+NH3 reaction over Fe-MFI with high Fe loading.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.