Abstract
The objective of the present work, is to assess the effect of tool material and cutting parameters on surface roughness of the supermet 718 Nickel-base superalloy, under dry cutting conditions and a constant nose radius (0.5 mm). The parameters investigated are cutting speed, feed rate, depth of cut and tool material. The tool materials used were the ceramic (Sandvik CC 680) and the CBN (Sandvik CB 50) inserts. These variables were investigated using a 2k factorial design. The present work demonstrates a favorable effect for ceramic inserts on surface roughness, when compared with CBN inserts. The work also, showed that the feed rate has the dominant effect among the parameters studied on the surface roughness, irrespective of the tool material used.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.