Abstract

The effect of the ratio CaO.Al2O3/12CaO.7Al2O3, AlF3 and CaF2 on the formation of the structure and phase composition of clinker minerals of aluminate cement during hydration has been studied. It is found that after 24 hours of hydration, the main hydraulic phases in the studied cement stones are CAH10, C2AH8, AH3. It has been shown that the introduction of AlF3 and CaF2 fluorides reduces the liquidus temperature of the systems and increases the rate of CA formation. Scanning electron microscopy has revealed that the process of hydration of calcium aluminates of cement at low temperatures can be considered as simultaneous reactions.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.