Abstract

AbstractPlastic deformation of the quasicrystalline decagonal phase Al72Co9Ni19, which appears macroscopically brittle at room temperature, has been performed by nanoindentation. Employing high resolution transmission electron microscopy it could be shown that near indents regions of a nanocrystalline phase appeared, which was identified as trigonal Al3(Ni,Co)2. So, for permanent deformation at room temperature no dislocation movement was needed. Instead, it seems reasonable to assume that the decagonal phase tends to decompose into a crystalline phase under stress. Values of nanohardness and elastic modulus determined during this work were found within the range of data reported so far by other authors. (© 2005 WILEY‐VCH Verlag GmbH & Co. KGaA, Weinheim)

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.