A new method for the oxidation protection of Ni-base superalloys with relatively low Al-content is proposed. By using the halogen effect the Al activity on the surface can be increased. Thus, the formation of a pure protective alumina scale becomes possible. The alloys IN738 and IN939 are considered in the present paper. Thermodynamic calculations for fluorine and chlorine predict the existence of the halogen effect for both alloys at temperatures between 900°C and 1200°C. The results also predict a change of the oxidation mechanism from internal alumina formation to external oxidation.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.