Abstract
The phase constitution of Ir–Nb–Zr alloys with a composition below 25 at% (Nb+Zr) was investigated by microstructure observation using scanning electron microscopy (SEM), composition analysis using electron probe microscopy analysis (EPMA), and phase identification using X-ray diffraction analysis (XRD). Partial isothermal sections of the Ir–Nb–Zr ternary system were determined at 1773, 2073, and 2373 K. It was found that the f.c.c. and L12 two-phase regions, which are shown in the Ir–Nb and Ir–Zr binary systems, were connected from the Ir–Nb side to the Ir–Zr side in the Ir–Nb–Zr ternary system. The potential of Ir–Nb–Zr alloys as high-temperature materials is discussed in terms of the microstructure and the lattice misfit between the f.c.c. and L12 phases.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.