Abstract
Magnetic hysteresis loop and ferromagnetic resonance (FMR) behaviour had been studied by considering the variation of the molar ratio of Li0.5−0.5x Ni x Fe2.5−0.5x O 4 ferrite nanostructure prepared by the hydrothermal method. The parameters of the ferrite nanostructure include coercivity (H c), saturation magnetisation (M s) and magnetic susceptibility. There was low coercivity at x = 0.3, high saturation magnetisation and high susceptibility (χ i) at (x = 0.5). These parameters showed an improvement in their values compared with the samples prepared by conventional methods. The FMR analysis indicated that these samples were lossy materials due to having a broad line width ranging from 800 to 925 G. The FMR lines had asymmetric shapes due to anisotropic broadening and conduction mechanism.