Abstract
Skim natural rubber (NR)–clay nanocomposites were prepared by a coagulation method using the organoclays Cloisite 15A, Cloisite 20A and Cloisite 30B. This work investigated the use of bagasse fiber developed from locally sourced and renewable material as an alternative and/or secondary filler in skim NR–clay nanocomposites. Bagasse fiber loading in the nanocomposites was 0, 5, 10 and 20 phr; the effects of fiber content on cure characteristics and mechanical properties were then determined. The results suggest that the Mooney viscosity tended to increase with increasing fiber content, whereas the cure time at 90% and fatigue testing score decreased as fiber loading increased.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.