Abstract
The effects of different pure Al compositon in the pack powder on aluminide coating formation of a new kind of Ni-Cr-W-Al nickel-base superalloy by pack cementation aluminizing was investigated. The content of pure Al powder is 15% and 30% in the aluminizing agent. The microstructure and phase composition of diffusion coating was studied.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.