Abstract

It is observed that for both UK and Japanese CR-39 detectors the mean diameters of fission fragment and alpha tracks from a Cf-252 source become larger as a result of UV exposure; but in the case of ‘UV exposure last’ (i.e. Cf + UV) the diameters are larger than in the case of ‘UV exposure first’ (i.e. UV + Cf). The bulk and track etching rates undergo an increase with UV exposure for the two kids of CR-39.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.