Abstract
The periodic morphology of cube shaped, coherent γ ′ [Ni3(Al, Ti)] precipitates in a representative nickel-base superalloy single crystal is shown to be influenced by the application of a 〈100〉 oriented uniaxial stress during annealing at elevated temperature. Furthermore, the stress annealed γ′ morphologies depend on the stress sense. Tensile and compressive stress annealing result in a directional coarsening of precipitates, and then agglomeration to form γ ′ precipitate plates with broad faces aligned perpendicular to the stress axis and precipitate parallelepipeds with long axes parallel to the stress axis, respectively. In explaining the morphological changes that occur during stress annealing, we consider two driving forces: i) a driving force due to changes in the stress-free shape of the specimen, and ii) a driving force due to changes in the effective modulus of the specimen. The first, which depends on a difference in the elastic constants and the lattice parameters of the two phases, is apparently the dominant driving force for the observed morphological changes in a stress annealed superalloy. The second, which depends only on a difference in elastic constants, may be important in alloys with elastically soft, incoherent inclusions such as pores.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.