Hydroxyapatite (HAp) is a vital material in various biomaterials but has low flexibility. Because of that, research has been done to increase the efficiency of hydroxyapatite by combining it with polyethylene glycol (PEG). HAp-PEG composite synthesis using blood cockle shell waste (Anadara granosa) as Ca precursor. The HAp-PEG composite was synthesized by in-situ to avoid high agglomeration. It was carried out with various temperatures to study the effect of temperature on the formation of the HAp-PEG composite and to determine the effect of temperature on its morphology and degradation properties. Fourier-Transform infrared (FTIR) characterization showed the presence of HAp and PEG functional group vibrations. X-Ray Diffraction (XRD) analysis showed that the composite had HAp peaks that matched the standard HAp ICSD #97849 and corresponded to pure PEG peaks. Characterization of Scanning Electron Microscopy-Energy Dispersive Spectroscopy (SEM-EDS) It is known that the synthesis temperature affects the morphology and hydroxyapatite ratio. Thermogravimetric Analysis-Differential Thermal Analysis (TGA-DTA) analyzed weight reduction in HAp-PEG composite samples, showing that the composite experienced a significant decrease in mass at 176–306, indicating PEG decomposition. The HAp-PEG composite degradation behavior test confirmed that the optimum temperature for degradation occurred at 70 ​°C.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.