Abstract

In this study, Ta powder was produced from Ta scarp via chemical processes using Mg and Ca powders. At first, Tantalum scraps were converted to Tantalum oxide (Ta2O5) at 1100˚C in an oxygen atmosphere. Tantalum oxide was reduced to Tantalum powder with Mg in a vacuum environment at 950 to 1200˚C for 3 hours. The obtained Ta powders further were reacted with Ca at 950˚C for 5 hours in a vacuum atmosphere. The powders were analyzed through X-ray diffraction patterns (XRD), scanning electron microscopy (SEM), as well as oxygen measurement. The results show that the average particles size of the produced Ta powders is about 58 nm with oxygen contents of 250 ppm.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.