Abstract
The SiC coating on C/C composites was prepared by CVD and pack-cementation method in this paper, then SiC coated C/C composites was jointed with LAS glass ceramic at 1423K for 30min and the pressure of 15 MPa. The structure and morphology of the SiC coating and as-received joints were analyzed by SEM and XRD; shear strength of joint was examined through the Instron universal testing tensile machine. The results show that the thickness of SiC coating prepared by CVD is about 30μm, while the thickness of SiC layer by pack-cementation is nearly 100μm, and the layer is easier to connect with LAS glass ceramic owing to the rough surface and wedge-shaped structure on the SiC coating; the shear strength of joint between SiC coating coated C/C and LAS by pack-cementation is greater than the joint of C/C- LAS with SiC coating prepared by CVD.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.