The microstructure and properties investigations silver powders consolidated by cyclic extrusion compression (CEC) were performed. The AgSnBi and AgNi powders using for electrical contacts were investigated. The observation by using optical microscopy (MO) and transmission electron microscopy (TEM) were apply. The strong diminishing of microstructure inside the consolidated granules were found. This phenomenon cause microhardness increase, restricted by material porosity.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.