Abstract

The paper presents selected aspects of the effect of primers on adhesive properties and strength of aluminium sheet adhesive joints, made using polyurethane adhesives. The strength of adhesive joints was determined based on two cure time variants: 15 and 64 h. It was found that the longer cure time at a humidity of 33% is more desired, as it leads to a substantial increase in strength of the tested adhesive joints. In addition, two variants of surface preparation were applied: degreasing and degreasing followed by the application of a primer (a pro-adhesive agent). It was observed that the primer application prior to the application of an adhesive leads to a significant increase in strength compared to the variant where the adhesive application is preceded only by degreasing. Moreover, the aluminium sheet surface that was subjected to cataphoretic painting and priming exhibits better adhesive properties. It has a higher value of both surface free energy and its dispersion and polar components compared to the surface that was only subjected to degreasing.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.