Abstract
Amorphous ribbons of Nb79Si21 were formed using the melt spinning technique. These were then implanted with nitrogen ions to form uniform surface layers of 1 and 2 at. % N. The A15 phase formed between annealing temperatures of 650–750 °C. The lattice parameter was 0.514 nm and the superconducting transition temperature was 6 K. To our knowledge, previous attempts to synthesize A15 Nb3Si from amorphous solids have required the application of very high pressures.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.