Abstract

Melt recycling Multilayer Packaging (MLP) waste is difficult due to challenging separation procedures. However, blending techniques with compatibilizers can simplify MLP waste melt recycling. PP-g-GMA is a common compatibilizer in polyolefin and PET blends. PP-g-GMA compatibilizer was synthesized by utilizing an internal mixer at 175℃, 50 rpm, and 10 min using styrene as a comonomer. Titration was a method to examine effect of three different sequences of adding the BPO initiator on GMA grafting. Each sequence's PP-g-GMA samples were compounded with MLP waste using a twin-screw extruder and injection molded to make tensile test specimens. FTIR analysis shows that the GMA and Styrene monomers had grafted onto the PP polymer backbone, with the GMA grafting degree by varying mixing sequence. Sequence 3, which introduced initiator, GMA, and styrene simultaneously to PP melt, yielded PP-g-GMA with the most significant GMA grafting degree of 5.11%. Adding PP-g-GMA produced from sequence 3 into the MLP melt enhanced the highest increase in tensile strength and elongation at break of the MLP/PP-g-GMA compound.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call