Abstract

Composites ZrB2‒CrB with a ceramic bond content of 80 wt. % and relative density 0,85‒0,90 were obtained by the method of electrothermal explosion (ETЕ) under pressure. It is shown that mechanical activation (MA) of the initial powder mixture reduces its heterogeneity and increases its reactivity. A fine ceramic composite with a homogeneous microstructure was obtained containing needle-like ZrB2 grains. Ill. 5. Ref. 13.

Full Text
Paper version not known

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.