Composite materials were prepared from C 3S and 12% (1) vinyl sulfonic acid (2) p-styrene sulfonic acid. The hydration of the composite systems were compared to that of neat C 3S for different ages up to 90 d, by DTA-TG, IR and XRD. The polymers were found to retard the hydration of the silicate due to the interaction between the Ca 2+ ions, released during the hydration of C 3S, and the sulfonate group of the polymers.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.