Cold bump pull tests performed on wafer level chip scale packages using SAC105 solder bumps show an increase in the occurrence of brittle failure modes with aging temperature and time. Fast intermetallic growth at 0–1000 h can be attributed to (Cu,Ni)6Sn5, while the decrease in intermetallic growth rate at t>1000 h can be attributed to diffusion processes leading to (Cu,Ni)6Sn5 and (Ni,Cu)3Sn4 formation and growth. Ni diffuses toward the solder bulk and saturates at 175–200°C, while Cu diffuses from the under bump metallization (UBM) toward the solder bump at 125–150°C. Interactions between Cu and Ni atoms lead to saturation of their atomic % gradients due to intermetallic formation. Sn diffusion from the solder toward the UBM occurs at 125–150°C. The activation energy for total intermetallic growth was calculated at 0.2 eV.

Talk to us

Join us for a 30 min session where you can share your feedback and ask us any queries you have

Schedule a call

Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.