Abstract
An electrochemical polarisation study has been conducted to determine the effect of impurity inclusions on the pitting corrosion behaviour of beryllium. Three grades of commercial beryllium differing in impurity levels were used. This work showed a strong relationship between the pitting potential of the beryllium and the level of impurity inclusions, the grade with the least number of overall inclusions being the most resistant to pitting corrosion. The work also revealed the preferred sites for pit initiation, with most corrosion pits initiating at intermetallic Fe/Al/Be inclusions, and to a smaller extent at inclusion sites containing either elemental silicon or carbides.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.