The influence of hydrogen content on the mechanical properties and size of dynamically recrystallized grains in commercially pure (CP) titanium and Ti-5Al-2.5Sn alloy was investigated. The alloys with hydrogen contents from 0.1 to 5.2 at.% were deformed in the a-field at temperatures of 650°, 750°С with initial strain rates of 5×10-4 s-1. A decrease of the deformation temperature leads to a reduction in grain size and to a stress increase for all compositions. This is in good agreement with the well known relation between the recrystallized grain size (d) and the steady flow stress ss=kd-n. At a given test temperature the steady state flow stress is four times lower and the grain size is about ten times greater in CP titanium in comparison with the Ti-5Al- 2.5Sn alloy. Hydrogen alloying of the Ti-5Al-2.5Sn alloy does not lead to a noticeable change in ss and d. However, an increase in hydrogen content from 0.1 to 5.2 at.% in CP titanium leads not only to a decrease in grain size by a factor of 2 but also to a decrease in flow stress (about 28%). This result is not in agreement with the above relation. This unusual behaviour may be due to two reasons: the influence of hydrogen on grain growth and the hydrogen effect on dynamic strain ageing. Both these effects are stronger in CP titanium.
Talk to us
Join us for a 30 min session where you can share your feedback and ask us any queries you have
Disclaimer: All third-party content on this website/platform is and will remain the property of their respective owners and is provided on "as is" basis without any warranties, express or implied. Use of third-party content does not indicate any affiliation, sponsorship with or endorsement by them. Any references to third-party content is to identify the corresponding services and shall be considered fair use under The CopyrightLaw.